Elution of monomer from different bulk fill dental composite resins
Yükleniyor...
Dosyalar
Tarih
2015
Dergi Başlığı
Dergi ISSN
Cilt Başlığı
Yayıncı
Elsevier Sci Ltd
Erişim Hakkı
info:eu-repo/semantics/closedAccess
Özet
Objective. The purpose of this study was to evaluate the elution of Bis-GMA, TEGDMA, HEMA, and Bis-EMA monomers from six bulk fill composite resins over four different time periods, using HPLC. Methods. Six different composite resin materials were used in the present study: Tetric Evo Ceram Bulk Fill (Ivoclar Vivadent, Amherst, NY), X-tra Fill (VOCO, Cuxhaven, Germany), Sonic Fill (Kerr, Orange, CA, USA), Filtek Bulk Fill (3M ESPE Dental Product, St. Paul, MN), SDR (Dentsply, Konstanz, Germany), EQUIA (GC America INC, Alsip, IL). The samples (4 mm thickness, 5 mm diameter) were prepared and polymerized for 20s with a light emitted diode unit. After fabrication, each sample was immediately immersed in 75 wt% ethanol/water solution used as extraction fluid and stored in the amber colored bottles at room temperature. Ethanol/water samples were taken (0.5 mL) at predefined time intervals:10 m (T1), 1 h (T2), 24h (T3) and 30 days (T4). These samples were analyzed by HPLC. The obtained data were analyzed with one-way ANOVA and Tukey HSD at significance level of p < 0.05. Results. Amount of eluted Bis-EMA and Bis-GMA from Tetric Evo Ceram Bulk Fill and amount of eluted TEGDMA and HEMA from X-tra Fill higher than others composites (p < 0.05). Significance. Residual monomers were eluted from bulk fill composite resins in all time periods and the amount of eluted monomers was increased with time. (C) 2015 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Açıklama
Anahtar Kelimeler
Bulk Fill Composite Resin, Elution, Residual Monomer, HPLC
Kaynak
Dental Materials
WoS Q Değeri
Q1
Scopus Q Değeri
Q1
Cilt
31
Sayı
7