Investigation of the effect of titanium alloy surface coating with different techniques on titanium-porcelain bonding
dc.authorid | 0000-0001-8890-2065 | en_US |
dc.contributor.author | Aslan, Muhammed Ali | |
dc.contributor.author | Ural, Çağrı | |
dc.contributor.author | Arıcı, Selim | |
dc.date.accessioned | 2021-06-23T19:44:52Z | |
dc.date.available | 2021-06-23T19:44:52Z | |
dc.date.issued | 2016 | |
dc.department | BAİBÜ, Diş Hekimliği Fakültesi, Protetik Diş Tedavisi Ana Bilim Dalı | en_US |
dc.description.abstract | Statement of Problem. The bond strength of dental porcelain to titanium is inadequate as a clinical alternative to conventional alloys for metal ceramic restorations. Purpose. The purpose of this in vitro study was to evaluate the effects of coating titanium surface with a micro-arc oxidation (MAO) technique and hydroxyapatite (HA) on the bond strength of porcelain to titanium surfaces. Material and methods. One hundred twenty machined titanium specimens with a dimension of 25x3x0.5 mm were prepared from grade 5 titanium as the metal substrate. Specimens were divided into 6 groups (n=20) according to the surface treatment used: airborne-particle abraded (control), coated with MAO for 5 minutes, coated with MAO for 15 minutes, coated with MAO for 30 minutes, coated with HA, and combination of MAO and HA. Each group was further divided into 2 subgroups (n=10) according to the type of porcelain used: Noritake Ti-22 porcelain or Vita-Titankeramik porcelain. The bond strength was tested with a universal testing machine at a crosshead speed of 0.5 mm/min. Data were analyzed statistically with 2-way ANOVA and Tukey honest significant differences multiple comparison tests (alpha=.05). Results. For both porcelain groups, the 30-minute MAO groups showed higher bond strength values than those of the control groups (P<.05). In the Vita Titankeramik porcelain subgroup, the specimens coated with HA- did not show any statistical differences compared with those of the control group (P>.05). Surface roughness was affected significantly (P<.001) by the coating procedure compared to that of the the control group. Conclusions. Coating with either MAO or HA improved titanium-porcelain adhesion. | en_US |
dc.identifier.doi | 10.1016/j.prosdent.2015.07.004 | |
dc.identifier.endpage | 122 | en_US |
dc.identifier.issn | 0022-3913 | |
dc.identifier.issn | 1097-6841 | |
dc.identifier.issue | 1 | en_US |
dc.identifier.pmid | 26412006 | en_US |
dc.identifier.scopus | 2-s2.0-84950156508 | en_US |
dc.identifier.scopusquality | Q1 | en_US |
dc.identifier.startpage | 115 | en_US |
dc.identifier.uri | https://doi.org/10.1016/j.prosdent.2015.07.004 | |
dc.identifier.uri | https://hdl.handle.net/20.500.12491/9059 | |
dc.identifier.volume | 115 | en_US |
dc.identifier.wos | WOS:000368044300019 | en_US |
dc.identifier.wosquality | Q2 | en_US |
dc.indekslendigikaynak | Web of Science | en_US |
dc.indekslendigikaynak | Scopus | en_US |
dc.indekslendigikaynak | PubMed | en_US |
dc.institutionauthor | Aslan, Muhammed Ali | |
dc.language.iso | en | en_US |
dc.publisher | Mosby-Elsevier | en_US |
dc.relation.ispartof | Journal Of Prosthetic Dentistry | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.rights | info:eu-repo/semantics/closedAccess | en_US |
dc.subject | Titanium-Porcelain Bonding | en_US |
dc.subject | Titanium Alloy Surface Coating | |
dc.subject | Dental Porcelain | |
dc.subject | Micro-Arc Oxidation (MAO) Technique | |
dc.title | Investigation of the effect of titanium alloy surface coating with different techniques on titanium-porcelain bonding | en_US |
dc.type | Article | en_US |
Dosyalar
Orijinal paket
1 - 1 / 1
Küçük Resim Yok
- İsim:
- muhammed-ali-aslan.pdf
- Boyut:
- 1.72 MB
- Biçim:
- Adobe Portable Document Format
- Açıklama:
- Tam Metin/Full Text