Özet

Purpose: To compare the effects of different thicknesses of ceramic veneering on the light transmission of various monolithic zirconia and lithium disilicate materials used in esthetic restorations. Methods: Zirconia (i.e., Katana UT, Katana HT, Prozir Diamond, Prozir HT, and Zenostar MO) and lithium disilicate specimens (i.e., Emax HT and Emax MO) were prepared at thicknesses of 0.5 mm, 0.8 mm, and 1.2 mm. Additionally, 0.8 mm-thick specimens and 0.3 mm-thick ceramic veneer were prepared for veneering groups. The total transmittance of light values were measured using a spectrophotometer. The light transmission values were analyzed using the Kruskal-Wallis and the post-hoc Dunnett tests (alpha= 0.05). Results: The Emax HT group defined significant differences from all groups (P< 0.05) at all thicknesses. The mean total transmittance of light ranged from 5.53% to 19.55%. There was no significant difference between the Katana UT and Prozir Diamond groups at the 0.5 mm, 0.8 mm, and 1.2 mm thicknesses (P> 0.05).

Açıklama

Anahtar Kelimeler

Zirconia, Katana UT, Katana HT, Prozir Diamond, Prozir HT, Emax HT

Kaynak

American Journal of Dentistry

WoS Q Değeri

Q3

Scopus Q Değeri

Q2

Cilt

36

Sayı

1

Künye

Koseler, E., Degirmenci, K., & Saridag, S. (2023). Comparison of the light transmission of new generation monolithic zirconia materials and lithium disilicate. American Journal of Dentistry, 36(1), 39-43.