Özet

An aqueous sol-gel synthesis route has been used for the preparation of undoped and cerium-doped strontium aluminate phase Sr4Al14O25. This study revealed required conditions for obtaining single phase compound, which are 1300 degrees C annealing temperature and addition of 2.5% of boric acid as a fluxing agent. The fact that boric acid is involved in the process of formation of strontium aluminate was confirmed by thermogravimetric measurements. A series of cerium-doped samples has been prepared and their excitation and emission spectra has been measured, which showed peaks at 330 nm and 385 nm, respectively. (C) 2014 Elsevier B.V. All rights reserved.

Açıklama

Anahtar Kelimeler

Strontium aluminate, Sr4Al14O25, Sol-gel synthesis, Cerium doping, Luminescence

Kaynak

Journal Of Alloys And Compounds

WoS Q Değeri

Q1

Scopus Q Değeri

Q1

Cilt

614

Sayı

Künye